Back to EFFICIENCY FINDER FOR METAL INDUSTRY
- Typical parameters of the process
Process | Temperature [°C] | Degreasing agent | Concentration [g/l] | Details | Literature |
Degreasing before tin plating | ~90 | Mixturs of polyphosphates, sodium hydroxide and wetting agents | 50-70 | BAT for the surface treatment of metals & plastics, 2006 |