- Typical parameters of the process
Process | Temperature [°C] | Heat transfer medium | Residence time | Chemicals | Concentration | Details | Literature |
Alkali phosphoting of aluminium | 40-70 (can be lowered to 25-35°C with special bath comeditions) | 5-10 sec | Aluminium, phosphate and fluoride solutions | 2-15 g/l | spaying of strip material | BAT for the surface treatment of metals & plastics, 2006 | |
1-3 min | spaying or dipping of individual parts |